项目 编号 | 5% SBS改性乳化沥青用量/% | CRL胶乳用量/% | FB用量/% |
C1 | 80 | 20 | 0 |
C2 | 80 | 20 | 0.3 |
C3 | 80 | 20 | 0.6 |
C4 | 80 | 20 | 0.9 |
C5 | 80 | 20 | 1.2 |
C6 | 80 | 20 | 1.5 |
C7 | 80 | 20 | 1.8 |
C8 | 80 | 20 | 2.1 |
C9 | 80 | 20 | 2.4 |