SRX含量(%) | 项目 | 饱水SRX稳定碎石试件干化后强度 | ||||
S0 | S1 | S2 | ...... | S5 | ||
0.25 | Rc (MPa) | 4.20 | 4.15 | 4.05 | ...... | 3.91 |
残留强度比 | 1.0 | 0.988 | 0.964 | ...... | 0.921 | |
0.50 | Rc (MPa) | 6.30 | 6.30 | 6.19 | ...... | 5.97 |
残留强度比 | 1.0 | 1.0 | 0.983 | ...... | 0.948 | |
0.75 | Rc (MPa) | 7.0 | 6.97 | 6.84 | ...... | 6.56 |
残留强度比 | 1.0 | 0.996 | 0.977 | ...... | 0.937 |