  |       Curing condition  |       PES loading in prepolymer (wt%)  |    ||
|   8  |       13  |       18  |    ||
|   tps (s)  |       Thermal curing (100˚C)  |       570  |       680  |       760  |    
|   Microwave curing (150˚C)  |       30  |       30  |       30  |    |
|   tgel (s)  |       Thermal curing (100˚C)  |       1010  |       940  |       860  |    
|   Microwave curing (150˚C)  |       223  |       213  |       205  |    |
|   K  |       Thermal curing (100˚C)  |       1.77/α  |       1.38/α  |       1.13/α  |    
|   Microwave curing (150˚C)  |       7.43/α  |       7.1/α  |       6.83/α  |    |