| Samples | BET (m2/g) | Craystal size (nm) | ||
| 500˚C | 900˚C | CuO | Co3O4 | |
| Co3O4 | 101 | 0.9 | - | 32.5 |
| 1Cu5Co | 119 | 2.5 | 31.3 | 27.6 |
| 1Cu2Co | 170 | 6.9 | 20.5 | 20.2 |
| 2Cu1Co | 145 | 4.1 | 27.4 | 22.9 |
| 5Cu1Co | 112 | 1.1 | 31.8 | 25.1 |
| CuO | 97 | 1.2 | 33.2 | - |