文献 | 催化剂种类 | 峰值电位(V, RHE) | 电流密度(A/mg) | 电活性表面积(m2/g) |
Li et al. [13] | Pt/C | 0.697 | 1.78 | 66.67 |
Lim et al. [14] | PtSn/C | 0.38 | 0.037 | 24.30 |
Li et al. [13] | PtRu/C | 0.647 | 3.37 | 56.50 |
Wang et al. [15] | PtNi3/C | 0.467 | 0.823 | 69.20 |
Hoseini et al. [16] | Pt/Pd薄膜 | 0.540 | 0.558 | 203.10 |
Hoseini et al. [16] | PtPd/RGO | 0.520 | 0.271 | 61.81 |
Ding et al. [17] | PtNi核–壳 | 0.544 | — | 50.08 |
Wu et al. [18] | Pt/RGO-SnO2 | 0.397 | 0.638 | 80.56 |
Wang et al. [52] | PtFeCo/C | — | 1.758 | 51.40 |
Yang et al. [19] | Cu@PtRu纳米线 | — | 0.45 | 29.00 |