Type | Test Method | Units | Gurit G-PETTM80 |
Density | ISO 845 | Kg/m3 | 80 |
Lb/ft3 | 5.0 | ||
Density Range | ISO 845 | Kg/m3 | 75-85 |
Lb/ft3 | 4.7-5.3 | ||
Compressive Strength | ASTM D1621-2010(ISO 844) | MPa | 0.96 |
Psi | 139 | ||
Compressive Modulus | ASTM D1621-2010(ISO 844) | MPa | 48 |
Psi | 6962 | ||
Compressive Modulus | ASTM D1621b-1973 | MPa | 77 |
Psi | 11168 | ||
Shear Strength | ASTM C273 | MPa | 0.53 |
Psi | 77 | ||
Shear Modulus | ASTM C273 | MPa | 13 |
Psi | 1885 | ||
Shear Elongation at break | ASTM C273 | % | 44 |
Tensile Strength | ASTM D1623 | MPa | 1.49 |
Psi | 216 | ||
Tensile Strength | ASTM D1623 | MPa | 89 |
Psi | 12908 | ||
HDT | DIN 53424 | ˚C | 200 |
˚F | 392 |