乳化沥青用量,% | 试件空隙率,% | 力值(KN) | 试件高度(mm) | 15℃劈裂抗拉强度(Mpa) |
3.0 | 11.4 | 14.04 | 100.73 | 0.59 |
3.5 | 11.7 | 15.47 | 100.86 | 0.65 |
4.0 | 11.5 | 16.64 | 99.6 | 0.71 |