材料状态 | 介质环境 | 断后伸长率 | 内积功 | 应力腐蚀敏感性指数 |
固溶态 | 空气 | 18.3% | 1480.5 | 27.3%*/35.2%** |
腐蚀溶液 | 13.3% | 958.9 | ||
应变强化4% | 空气 | 12.8% | 1026.4 | 40.6%/54.5% |
腐蚀溶液 | 7.6% | 467.3 | ||
应变强化8% | 空气 | 12.7% | 1157.5 | 69.3%/66.4% |
腐蚀溶液 | 3.9% | 388.8 |